Technical Specification
Hardness After Hardening & Tempering: HB280-320
Nitrided Hardness: HV900-1050
Nitrided Case Depth: 0.50-0.80mm
Nitrided Brittleness: Less than Grade 2
Surface Roughness: RA 0.4
Screw Straightness: 0.015mm
Surface Chromium-Plating's Hardness After Nitriding: ≥ 900HV
Chromium-Plating Depth: 0.025-0.10mm
Alloy Hardness: HRC55-65
Alloy Depth: 0.8-2.0mm